In-house melting and AOD refining let the foundry pour to a customised composition rather than a stock analysis. In-house testing then proves what was poured.

100+ ferrous alloys30+ nickel alloysAOD refinedPT / RT / UT in house

3.1Melt quality

Refined before it is poured.

Argon oxygen decarburisation removes carbon while protecting chromium, and takes phosphorus and sulphur down with it. That is why the foundry can pour super low carbon steels, duplex and super duplex grades and nickel-based steels with the cleanliness their corrosion performance depends on.

Very low carbon, phosphorus and sulphur contents are available on request, with chemistry customised to the order.

3.2Alloy families

Six families. Grades named the way your specification names them.

Designations below are those listed by the manufacturer. Material standards referenced include GB, ASTM, AISI, EN, DIN, BS, JIS, NF, AS, AAR. The grade and governing standard are confirmed in every quotation.

01Ferritic-austenitic

Duplex

The workhorse for rotating separation equipment. Compared with austenitic grades, the manufacturer points to higher strength and better resistance to intergranular and chloride stress corrosion; compared with ferritic grades, higher toughness and better weldability.

  • 2205 · EN 1.4462 · UNS S32205 / S31803
  • 2304 · EN 1.4362 · UNS S32304
  • 2101
  • S32003
02High-alloy duplex

Super duplex

For chloride-rich and sea-water duty where pitting resistance has to go further. Poured from AOD-refined melts with very low carbon, phosphorus and sulphur.

  • 2507 · EN 1.4410 · UNS S32750
  • S32707
  • S32760
03Corrosion-resistant

Austenitic

Standard and low-carbon austenitic grades for general corrosive service, widely used for bowls, scrolls, pipes and valve castings.

  • 304 / 304L
  • 316 / 316L
  • 904L
  • 347
04High strength

Martensitic and PH

Hardenable stainless steels for end hubs, roll shells and structural parts where strength and wear resistance lead the specification.

  • CA15
  • AISI 410
  • AISI 431
  • EN 1.4418
  • 17-4PH
05Elevated temperature

Heat-resistant

Steels for hot-section turbine casings, gratings and furnace-side parts, matched to the temperature zone the component works in.

  • F91
  • 309S
  • 310S
06Special alloys

Nickel-based

Nickel-based and high-nickel alloys for the most aggressive media and for hot gas paths. The manufacturer cites more than 30 nickel alloys in its portfolio.

  • Ni-Cr-Mo alloys
  • Hastelloy alloys
  • CN7M

3.3Selection by duty

Where the manufacturer points each grade.

DutyMediumGrades indicated
Decanter bowls and scrollsWaste water, oil sludge, mining mud, palm oil: corrosive and abrasiveDuplex 2304 or 2205; austenitic 304 or 316
Pulp bleaching equipmentChloride and acid with chlorine and chlorine dioxide. 316L is not suitable at the chlorination tower top or pulp washerDuplex 2101, 2304, 2205
Suction roll shellsPaper machine wet endDuplex 2304 (EN 1.4362) or 2205 (EN 1.4462)
Gas turbine outer casingsHot-section structure at high temperature and pressureHigh-chromium martensitic heat-resistant steel
Gas turbine stator ringsHot gas path, oxidation and corrosionNickel-based Ni-Cr-Mo alloy
Sea-water and chemical pumps and valvesChlorides, chemicals, oilsDuplex and super duplex grades; special alloys to specification

Indications taken from the manufacturer’s application notes. Final material selection rests with the equipment designer.

3.4Accuracy and surface

What to expect from the casting, and from the machined part.

Published values for the standard range. Roll shells are listed at CT8 to CT12 with a machined finish of Ra 3.2 µm.

Casting tolerance gradeCT9 to CT12

finercoarser

Surface roughness Ra, µmlogarithmic scale

3.5Inspection and testing

Checked throughout production, not only at the end.

Testing is carried out in house. The scope applied to an order, including acceptance levels and documentation, is agreed at quotation.

  • CA

    Chemical analysis

    Melt and product chemistry checked against the ordered grade.

  • MT

    Mechanical and physical properties

    Property tests on the heat-treated material.

  • PT

    Penetrant testing

    Surface-breaking indications on cast and machined faces.

  • RT

    Radiographic testing

    Internal soundness of the wall and critical sections.

  • UT

    Ultrasonic testing

    Volumetric examination of heavy sections.

  • DI

    Dimensional inspection

    Checks against the drawing through production.

  • CMM

    Three-coordinate measurement

    Coordinate measurement of machined features.

  • 3D

    3D scanning

    Full-surface comparison of the casting with its model.

3.6Management systems

Certified systems behind the product.

The manufacturer holds the certificates listed here and was a main drafter of JB/T 11874-2014, the Chinese machinery industry standard for centrifugally cast stainless steel cylinders for separation machinery.

  • ISO 9001:2015Quality management system
  • ISO 14001:2015Environmental management system
  • ISO 45001:2018Occupational health and safety management system
  • ISO 19600:2014Compliance management system
  • CECertificate for centrifugally cast stainless steel
  • GB/T 29490-2013Intellectual property management system